MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metalmen Sales
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Sheet and Strip, UNS N07718
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to approximately 982 degrees Celsius. In addition, the alloy exhibits excellent tensile and impact strength even at cryogenic temperatures. High strength at room and elevated temperatures is developed by a precipitation heat treatment at 718 degrees Celsius with cooling and a hold at 621°C.

The relatively slow response to precipitation hardening permits repair welding of the Altemp 718 alloy even in the aged condition. The Altemp 718 alloy is usually produced by a double melt practice using consumable electrode remelt procedures to provide homogeneity and extremely clean structures. Specific uses include aircraft ducting and engine plumbing.

Tensile properties below are from AMS 5596 and/or AMS 5597.

Information provided by Allegheny Ludlum

Key Words: DIN 2.4668; ASTM B-670; AMS 5596; AMS 5597
Vendors:
Available Properties
  • Density
  • Hardness, Rockwell B, Typical Annealed
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break, in 2"
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air, oxidation resistance to this temp
  • Aluminum, Al
  • Boron, B
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Copper, Cu
  • Iron, Fe, as balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Niobium, Nb (Columbium, Cb)
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ATI Allegheny Ludlum, Allegheny Technologies Incorporated

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metalmen Sales
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.