MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger SPI
Ensinger TECASINT 5501 ESD light-brown Polyimide, Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Glass Fiber

Material Notes:
  • electrically static dissipative
  • high thermal and mechanical capacity
  • low thermal expansion
  • high creep resistance
  • resistance against high energy radiation
Target Industries:
  • electronics
  • semiconductor technology
  • cryogenic engineering
  • electrical engineering
  • mechanical engineering
  • nuclear and vacuum technology

Information provided by Ensinger Inc.

Vendors:
Available Properties
  • Density
  • Water Absorption, DIN EN ISO 62
  • Hardness, Rockwell M, ISO 2039/2
  • Hardness, Shore D, DIN EN ISO 868
  • Tensile Strength, DIN EN ISO 527-1, 50 mm/min
  • Elongation at Break, DIN EN ISO 527-1, 50 mm/min
  • Modulus of Elasticity, DIN EN ISO 527-1, 1 mm/min
  • Flexural Strength, DIN EN ISO 178, 10 mm/min
  • Flexural Modulus, DIN EN ISO 178, 2 mm/min
  • Flexural Strain at Break, DIN EN ISO 178, 10 mm/min
  • Compressive Strain at Break, EN ISO 604, 10 mm/min
  • Compressive Strength, EN ISO 604, 10 mm/min
  • Charpy Impact Unnotched, DIN EN ISO 179-1, max 7.5 J
  • Volume Resistivity, DIN EN 61340-2-3
  • Surface Resistance, DIN EN 61340-2-3
  • CTE, linear, DIN 53 752, XY
  • CTE, linear, DIN 53 752, XY
  • CTE, linear, DIN 53 752, XY
  • Specific Heat Capacity, DIN EN 821
  • Thermal Conductivity, DIN EN 821
  • Maximum Service Temperature, Air, short-term
  • Glass Transition Temp, Tg, DIN EN ISO 11357
  • Flammability, UL94, DIN IEC 60695-11-10
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.