MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Chesterton 625 CXF Corrosion Resistant, Extreme Pressure Grease -Food Grade
Categories: Fluid; Lubricant

Material Notes: Description: Superior resistance to washout by water, caustics, sanitizing cleaners, process fluids and steam has been combined with high purity USP White Mineral OIl to produce Chesterton® 625 CXF suitable for Food, Beverage and Pharmaceutical use. As a premium quality, water resistant grease, 625 will not be removed even in severe water washout situations. With a dropping point of 318°C (604°F), it will not melt and run out within recommended operating parameters. 625 is NSF Registered H1 and complies with FDA regulations 178.3570. It can be the exclusive lubricating grease used in food, beverage, meat, poultry and pharmaceutical plants. Chesterton 625 CXF is virtually non-staining. Grease stains on floors and packaging equipment can be substantially reduced. Use 625 to lubricate packaging machinery and paper converting equipment. Chesterton 625 CXF is essentially tasteless and odorless. It is ideal as a maintenance or production lubricant used in food processing equipment, mixing, filling, packaging and production machinery. Chesterton 625 contains no animal fats or oils which could become rancid and support biological growth. Further, it contains no heavy metals which could mandate hazardous warnings and restrict use.

Features:

  • Virtually impervious to water and steam
  • USP White Oil Base Fluid
  • Smooth, Buttery Texture
  • Adheres to Metal
  • Water and Corrosion resistant
  • NSF H! - Registration number 138414
  • FDA Compliant
  • Virtually Tasteless and Odorless
  • Speed Rating, DN to 500,000

Suggested Uses: Use in all applications where conventional greases break down under shear, thermal abuse, shock loading and water contaminating. Chesterton 625 CXF can be used wherever food-grade grease is required.

Applications:

  • Lubrication of slides, guides, plain bearings and bushings
  • All types of anti-friction bearings, roller bearings and ball bearings
  • Grease-lubricated chains
  • Gears and cams
  • Motor Operated Valves
  • Couplings, joints and splined shafts
  • And other moving parts of equipment used in the manufacture of food, drugs, cosmetics, beverages such as: bottle and carton fillings, Paste and sauce fillers, Conveyer belts and rollers, Feeders, mixers and agitators and Canning machines, seamers.

Lubricating Additives: Non Heavy Metal, Extreme Pressure and Anti-Wear, Anti-Fretting Additives, Surface Reactive Anti-Rust and Corrosion Additives, Oxidation Inhibitors

Information provided by Chesterton

Vendors:
Available Properties
  • Specific Gravity
  • Viscosity Measurement, ASTM D445, Base Oil
  • Kinematic Viscosity at 40°C (104°F), ASTM D445, Base Oil
  • Kinematic Viscosity at 100°C (212°F), ASTM D445, Base Oil
  • Four Ball Extreme Pressure, Load Wear Index, ASTM D2596, DIN 51 350/4
  • Four Ball Extreme Pressure, Weld Load, ASTM D2596, DIN 51 350/4
  • Four Ball Wear, ASTM D2266, DIN 51 350/5, 1200 rpm, 40 kg, scar diameter
  • Penetration, ASTM D217, DIN ISO 2137
  • Oil Separation, ASTM D1742, loss
  • Timken Test, ASTM D2509
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Dropping Point, ASTM D2265, DIN 51 801/1
  • FDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.