| GUARD DOG™ UV123 hindered amine light stabilizer is highly effective in protecting polymers against degradation caused by exposure to UV radiation. Applications: GUARD DOG™ UV123 is mainly used in Coatings, Printing Ink, Liquid Color Concentrates, Polyolefins, Polyurethane, Sealants, Adhesives, Elastomers, Unsaturated Polyesters, Acrylics and Styrenics. This stabilizers protects automotive coatings from UV degradation. it also exhibits synergy when used in combination with benzotriazole absorbers. Typical Properties: - Product Form - Yellow viscous liquid
- Monomer content - 65% minimum (based on LC assay)
- Dimer content - 20% maximum (based on LC assay)
|