MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Eastman Foralyn™ 110 Ester of Hydrogenated Rosin
Categories: Other Engineering Material

Material Notes: Product Description: Foralyn™ 110 Ester of Hydrogenated Rosin is the pentaerythritol ester of hydrogenated rosin. This resin combines the feature of light initial color and good color retention with the advantages of excellent long-term retention of adhesive properties and UV light stability offered by Staybelite™ and Foral™ Esters of Hydrogenated Rosin.

Application/Uses:

  • Automotive
  • Building and Construction
  • Caulks and Sealants
  • Contact Adhesives
  • Hot Melt Adhesives
  • Laminating
  • Nonwovens
  • Packaging
  • Pressure sensitive adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Tapes and Labels
  • Wax Modification
Key Attributes:
  • Excellent resistance to oxidation
  • High softening point
  • Light color
  • Low odor
  • Thermoplastic hydrogenated resin
  • Wide solubility and compatibility rangeInformation provided by Eastman
Vendors:
Available Properties
  • Density
  • Viscosity, Melt
  • Viscosity, Melt
  • Viscosity, Melt
  • Total Acid Number, [mg KOH/g]
  • Ring & Ball Softening Point, ASTM E 28
  • Gardner Color Number
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.