Source: Mouse Quality: Tested for ability to initiate neurite outgrowth of NG-108 human neuroblastoma cells; Found negative for bacteria, fungi, and mycoplasma Application: This is entactic free and is used as a thin coating on tissue-culture surfaces or as a soluble additive to culture medium. Laminin is a major component of basement membranes. It has numerous biological activities including promotion of cell adhesion, migration, chemotaxis, growth, and differentiation, including neurite outgrowth. Information provided by Matexcel |