MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Trinseo INSPIRE™ TF1500 ESU Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Talc filled, high impact PP compound. INSPIRE™ TF1500 ESU has been developed for aesthetic automotive applications, with good scratch resistance and UV light stabilization. It is especially suitable for car interior applications requiring ductility, because of its high impact resistance, even at low temperatures.

Application areas:

  • Instrument panel retainer
  • Instrument panel trim
  • Midconsole
  • Door panels
  • Door pockets
  • Interior trim
  • Trunk trim
Automotive Specifications:
  • GM QK 004022 U Color: Charcoal
  • PSA Peugeot-Citroen SPA 3858
  • IMDS ID 21758150 Color: Charcoal
Information provided by Dow

Vendors:
Available Properties
  • Density
  • Filler Content, Talc
  • Melt Flow, ISO 1133
  • Tensile Strength, Yield, ISO 527, 50mm/min
  • Elongation at Break, ISO 527, 50 mm/min
  • Tensile Modulus, ISO 527, 1 mm/min
  • Flexural Modulus, ISO 178, 3 points and 2 mm/min
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Izod Impact, Notched (ISO), ISO 180/1A
  • CTE, linear, ASTM D696
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75, Unannealed
  • Vicat Softening Point, ISO 306 A
  • Shrinkage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Trinseo, former Styron

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.