MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Envalior Durethan® BKV 30 H2.0 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistance

Application Examples: pedal brackets, automotive front end structures

Former Lanxess product line is now with Envalior.

Vendors:
Available Properties
  • Bulk Density, ISO 60
  • Density, ISO 1183
  • Moisture Absorption at Equilibrium, ISO 62, 50% RH
  • Water Absorption at Saturation, IOS 62
  • Linear Mold Shrinkage, Flow, ISO 294-4, 60x60x2; 280 °C / MT 80°C; 600 bar
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 60x60x2; 280 °C / MT 80°C; 600 bar
  • Puncture Resistance, ISO 6603-2
  • Puncture Resistance, ISO 6603-2
  • Ball Indentation Hardness, ISO 2093-1
  • Tensile Strength at Break, ISO 527-1,-2, 5 mm/min
  • Elongation at Break, ISO 527-1,-2, 5 mm/min
  • Tensile Modulus, ISO 527-1,-2, 1 mm/min
  • Flexural Strength, ISO 178-A, 2 mm/min
  • Flexural Yield Strength, ISO 178-A, 2 mm/min
  • Flexural Modulus, ISO 178-A, 2 mm/min
  • Flexural Strain at Break, ISO 178-A, 2 mm/min
  • Izod Impact, Notched (ISO), ISO 180-1A
  • Izod Impact, Notched (ISO), ISO 180-1A
  • Izod Impact, Unnotched (ISO), ISO 180-1U
  • Izod Impact, Unnotched (ISO), ISO 180-1U
  • Charpy Impact Unnotched, ISO 179-1eU
  • Charpy Impact Unnotched, ISO 179-1eU
  • Charpy Impact, Notched, ISO 179 1eA
  • Charpy Impact, Notched, ISO 179 1eA
  • Puncture Energy, ISO 6603-2
  • Puncture Energy, ISO 6603-2
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, IEC 60112, Solution A
  • CTE, linear, Parallel to Flow, ISO 11359-1,-2
  • CTE, linear, Transverse to Flow, ISO 11359-1,-2
  • Melting Point, ISO 11357-1,-3, 10°C/min
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1,-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1,-2
  • Vicat Softening Point, ISO 306, 120°C/h
  • Vicat Softening Point, ISO 306, 50°C/h
  • Flammability, UL94
  • Flammability, UL94
  • Oxygen Index, ISO 4589-2, Method A
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Shrinkage, MD, ISO 294-4, Post-Shrinkage Flow Direction; 60x60x2
  • Shrinkage, TD, ISO 294-4, 60x60x2
  • Melt Temperature, injection molding
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  • Moisture Content, Karl Fischer
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Envalior, former LANXESS

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.