Hifax TYC 1342P YBTA Platinum very high melt flow, 1,650 MPa flexural modulus, low density mineral filled, thermoplastic elastomeric olefin (TEO) resin. Enables part weight reduction and associated savings while maintaining all of the performance of traditional, higher density products. It has excellent UV performance, balance of properties and processability, and is typically used for MIC automotive bumper fascias and exterior trim applications. Availability: North America Application: Automotive Parts; Bumpers; Exterior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Good Dimensional Stability; Good Processability; High Impact Resistance; Low Density; Low Shrinkage; UV Resistant Information provided by LyondellBasell. |