MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Chesterton ARC 5ES Rapid Repair Adhesive Stick
Categories: Polymer; Thermoset; Epoxy

Material Notes: ARC 5ES is specifically formulated for quick reliable repairs. Its “stick” design combines the performance of a two component system with the convenience of a single component. The ARC 5ES is kneaded by hand to mix the components, which are then simply applied to the surface to be repaired. The 5ES hardens in 5-7 minutes and cures to full strength in 30 minutes. Its putty like consistency and moisture insensitive chemistry resist washout when repairing leaks. Cures under water, bonds to wet surfaces, 100% solids, non-shrinking.

Benefits:

  • Once cured, seals 3 mm (1/8”) leaks up to seven atmospheres (100 psi).
  • Putty like viscosity resist washout when sealing leaks
  • Bonds and cures under water
  • Tough resin structure resists thermal mechanical shock
  • Labor and down time are reduced due to ease of use and rapid curing
  • Convenient packaging is easily carried in pocket or tool box
  • Color change verifies complete mix
  • Cures down to 4°C (40°F)
  • Benchmark tested to be the best available technology for leak repairs
  • ARC 5ES is certified by NSF to NSF/ANSI Standard 61.

Suggested Uses:

    Stop Leaks:
  • Pipes
  • Air Ducts
  • Fiberglass
  • Conduits
  • Radiators
  • Valves
  • Pumps
  • Pools
    Repair:
  • Cracked Battery Casings
  • Lavatory Fixtures
  • Cracked Tile & Marble
    Fasten or Adhere:
  • Signs
  • Temporary Fixtures

Information provided by Chesterton

Vendors:
Available Properties
  • Density
  • Hardness, Shore D
  • Compressive Strength, ASTM D695
  • Adhesive Bond Strength, ASTM D1002, Unclean
  • Adhesive Bond Strength, ASTM D1002, SSPC SP3-Wet
  • Adhesive Bond Strength, ASTM D1002, SSPC SP3-Dry
  • Dielectric Strength, ASTM D149
  • Maximum Service Temperature, Air, Wet
  • Maximum Service Temperature, Air, Dry
  • Cure Time, Cure Time to 90% Shore D
  • Cure Time, Initial Set
  • Cure Time, Initial Set
  • Cure Time, Initial Set
  • Cure Time, Full Chemical
  • Cure Time, Full Chemical
  • Cure Time, Full Chemical
  • Cure Time, Full Chemical
  • Cure Time, Initial Set
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.