MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ChevronTexaco Aquagear® EP 460
Categories: Fluid; Lubricant

Material Notes: Texaco Aquagear EP oils deliver value through:
  • Long equipment life — Effective sulfur-phosphorus extreme-pressure additives provide high film thickness that protects gear teeth from wear and premature failure.
  • Long oil life — Special additives and base oil formulations prevent product degradation when operating in severe conditions that lead to rapid oxidation and thermal stress — providing long service life of the oil.
  • Flexibility to use in wet conditions — Quickly forms stable emulsions with water to prevent separated water from corroding equipment, and reduces water corrosion on either steel (rust) or nonferrous metals (including copper and its alloys) in gear sets.
  • Cold weather reliability — Pour point is depressed to provide good cold flow performance at low temperature conditions.

Texaco Aquagear EP oils are multipurpose gear lubricants.

They are formulated with highly refined, high viscosity index paraffinic base oils and a new generation sulfurphosphorus additive system. Texaco Aquagear EP oils contain extreme pressure, antiwear and emulsibility additives; oxidation, rust, corrosion and foam inhibitors; a pour point depressant; and a metal deactivator to protect copper or copper alloys from corrosion.

They are specifically designed to meet or exceed the performance requirements of Joy Technologies specifications for transmission oils.

Texaco Aquagear EP oils high film strength and load-carrying capacity. Gear teeth are protected from wear, all types of surface distress, and premature failure.

They provide improved thermal and oxidation stability to prevent degradation under severe operating conditions and provide longer lubricant life.

They are designed to form a stable emulsion with contaminating water.

Texaco Aquagear EP oils are recommended for use in Joy Technologies transmissions or other similar applications where water emulsifying gear oils are required.

Texaco Aquagear EP oils meet Joy specifications TO-MEP (ISO 220), TO-HEP (ISO 320) and TO-HD (ISO 460).

Texaco Aquagear EP oils can be used in industrial applications where overloading, severe operating conditions, high lubricant operating temperatures, or other problems are encountered.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222684; MSDS Number: 8641

Vendors:
Available Properties
  • API Gravity
  • Viscosity Measurement, ASTM D2893, Viscosity Oxidative % Increase
  • Viscosity Measurement, Viscosity Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Falex Load Test, ASTM D3233, EP
  • Pour Point
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.