MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Parker Chomerics CHO-THERM® 1671 High Power Thermally Conductive Electrical Insulator Pad
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: CHO-THERM® high-power thermal insulator pads are thermally conductive materials designed for use where the highest possible thermal, dielectric, and mechanical properties are required. Fiberglass cloth reinforcement strengthens CHO-THERM® pads against tear, cut-through and punctures. These materials are available in sheet form and die-cut configurations. An optional acrylic adhesive layer (with PSA) is available on one or two sides. With a proven track record spanning several decades in multiple applications, these products are the first choice for high-end power supplies, industrial, aerospace, and military/avionics applications.

Features/Benefits: Excellent thermal properties, High dielectric strength, Excellent mechanical strength and puncture resistance, 100% inspected for dielectric properties on every sheet, PSA attachment option available, Meets RoHS specifications, and Proven through decades of use in demanding military and aerospace applications.

Typical Applications: Power conversion equipment, Power supplies and UPS, Power semiconductors, Automotive electronics, Motor and engine controllers, and Televisions and consumer electronics

Product Attributes: Economically-priced and Low thermal impedance

Information provided by Chomerics

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Thickness, ASTM D374
  • Outgassing - Total Mass Loss, ASTM E595, TML
  • Collected Volatile Condensable Material, ASTM E595
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, ASTM D412
  • Elongation at Break, ASTM D412
  • Tear Strength, ASTM D642
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Breakdown, ASTM D149
  • Dissipation Factor, Chomerics Test
  • CTE, linear, ASTM E831
  • Specific Heat Capacity, ASTM E1296
  • Thermal Conductivity, ASTM D5470
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Shelf Life, Chomerics, Months for shipment, with PSA
  • Shelf Life, Chomerics, Months for shipment, Dry Pad
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.