MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Chemical Concepts Chem-Set™ CCS-RTV6500 Hi Temp Red Silicone
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Heat Resistant Sealant is a one-part, nonslumping paste that cures to a rubbery solid at room temperature on exposure to water vapor in the air. This silicone product is formulated to perform at temperatures ranging from -65 to 260º (-85 to 500ºF) for continuous operation and to 315ºC (600ºF) for intermittent exposure. It can be used for numerous sealing and bonding applications. Non-slumping sealant designed for sealing and bonding applications: exposed to temperatures as high as 315°C (600°F).

APPLICATIONS: The high temperature properties of this sealant make it ideally suited for:Sealing and encapsula and protective coatings, where parts must perform at high temperatures.

Information provided by Chemical Concepts™.

Vendors:
Available Properties
  • Specific Gravity
  • Hardness, Shore A, cured after 72 hrs & 50% RH
  • Tensile Strength, cured 72 hrs, @ 25°C, & 50% RH
  • Elongation at Break, Cured 72 hrs @ 25°C, & 50% RH
  • Maximum Service Temperature, Air, continuous
  • Maximum Service Temperature, Air, intermittent
  • Minimum Service Temperature, Air, continuous
  • Extrusion Rate, 1/8 inch orifice, @ 90 psi
  • Cure Time, 1/8 inch thickness, 50% RH
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.