MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Atom Adhesives AA-DUCT 905 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-DUCT 905 is a single component epoxy, formulated with pure silver powder combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive substrates. AA-DUCT 905 shows slight settling when stored for a long period of time, no caking and will re disperse to a smooth homogeneous state. AA-DUCT 905 formulation produces electrically conductive paths on a wide variety of surfaces including plastics, rubber, cloth, thermoplastic, paper, wood and many others. AA-DUCT 905 is designed for use in diversified applications such as microwave EMI & RFI shielding, in the assembly or repair of printed circuit boards, wave-guides, electronic modules, flat cable, static shielding, connections and circuitry. This epoxy is designed for screening and micro product adhesion applications with the best dispensing capabilities of up to 30 gauge / 0.01"/ 0.255mm.

Appearance: Silver

Cure Type: Heat cure

Benefits:

  • High strength
  • Perfect bond
  • EMI&RFI shielding
  • Wave guides
  • The best dispensing capabilities of up to 30 gauge/0.01”/0.255mm
Substrates: Integrated circuits, aluminum, copper, magnesium, steel, bronze, nickel, kovar, ceramic, glass, phenolic and G-10 epoxy glass boards.

Catalyst: Anhydride

Information provided by Atom Adhesives

Vendors:
Available Properties
  • Specific Gravity, Uncured
  • Viscosity, Uncured
  • Hardness, Shore D
  • Tensile Strength, Adhesion
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Strength, Lap
  • Volume Resistivity
  • Surface Resistivity per Square
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Cure Time
  • Pot Life, uncured
  • Shelf Life, uncured
  • Silver, Ag
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.