MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Trelleborg Sealing Solutions Turcite® TX Self-Lubricating Thermoplastic Rod
Categories: Polymer; Thermoplastic

Material Notes: Red color. Turcite® TX is engineered to handle moderate load, high speed applications. It exhibits an excellent surface finish when machined. It has a long service life and exceptionally low coefficient of friction and high PV.

General Turcite® information: Exhibit excellent wear resistance, durability, and no slip-stick under oscillating motion. Axial-loaded shafts benefit from reduced friction. Uses include transmissions, home appliances, bicycles, food processing equipment, exercise equipment, rotating displays, and caster assemblies.

Informatiuon provided by Busak + Shamban, now Trelleborg Sealing Solutions.

Busak+Shamban changed its name to Trelleborg Sealing Solutions in 2007.

Key Words: Busak + Shamban; TI Group; Smiths Group
Vendors:
Available Properties
  • Water Absorption
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Coefficient of Friction, non-lubricated
  • K (wear) Factor
  • Limiting Pressure Velocity
  • CTE, linear
  • Maximum Service Temperature, Air, Continuous
  • Maximum Service Temperature, Air, Deflection Temperature with load unspecified
  • Maximum Service Temperature, Air, Intermittent
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Trelleborg Sealing Solutions (Smiths Group)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2026 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.