MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
PBI Performance Products S26 Thermal Resistant Polybenzimidazole Solution
Categories: Fluid; Polymer; Thermoplastic; Polybenzimidazole (PBI)

Material Notes: Polybenzimidazole (PBI) solutions are suitable products for film casting, dip coating, spray coating and resin impregnation. PBI can be firmly adhered to steel, stainless steel, aluminum, copper, nickel- chromium, glass, ceramics and plastics. PBI coatings are highly resistant to heat and chemical attack. PBI will provide electrical insulation and wear resistance.
S26 is a solution containing nominally 26% w/w PBI solids in conjunction with 1.5% w/w LiCl salt in dimethylacetamide (DMAc) to  form a 2100 Poise solution. This grade is easily thinned and can be used for films or coatings.
The LiCl stabilizer imparts long shelf life and can be easily removed with an 85°C, 1-hour, aqueous wash of a thin film.

Information provided by PBI Performance Products

Vendors:
Available Properties
  • Solids Content
  • Water Absorption, ASTM D570, for bulk PBI
  • Viscosity, 5% PBI Solids
  • Viscosity, 10% PBI Solids
  • Viscosity, 15% PBI Solids
  • Viscosity, 20% PBI Solids
  • Viscosity, 25% PBI Solids
  • Viscosity, as supplied S26 solution
  • Viscosity, as supplied S26 solution
  • Tensile Strength, ASTM D638, for bulk PBI
  • Elongation at Break, for bulk PBI
  • Tensile Modulus, for bulk PBI
  • Dielectric Constant, ASTM D150, for bulk PBI
  • Dielectric Strength, ASTM D149, for bulk PBI
  • Dissipation Factor, ASTM D150, for bulk PBI
  • CTE, linear, ASTM TMA, for bulk PBI
  • Glass Transition Temp, Tg, ASTM DMA, for bulk PBI
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
PBI Performance Products, Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.