MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Omnia Plastica PC Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: This amorphous polymer is commonly used for its high shock resistance even at low temperature. It is not a material recommended for mechanical applications, even if its dimensional stability does make it suitable for precision parts.

Features:

  • Clear Shock resistance
  • Dielectric properties
  • Dimensional stability
  • Colour: clear
Weak Point:

It has no self-lubricating power and it is attacked by oil and grease, therefore it cannot be considered suitable for lubricated moving mechanical parts.

Application:

  • Electrical : good dielectric properties. It is mainly used in this field.
  • Chemical: the use of PC in the chemical industry is not ideal, due to the poor resistance to hydrocarbons.
  • Food contact: physiologically inert if natural.
  • Mechanical: it is used for precision mechanisms when good dimensional stability is required.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Vendors:
Available Properties
  • Density, ISO.1183 DIN.53479
  • Moisture Absorption at Equilibrium, 50% relative humidity
  • Water Absorption at Saturation, 23°C
  • Hardness, Rockwell M, ISO2039.2, dry sample
  • Ball Indentation Hardness, ISO2039.1 DIN.53456
  • Tensile Strength at Break, ISO.527 DIN.53455
  • Elongation at Break, ISO.527 DIN.53455
  • Tensile Modulus, ISO.527 DIN.53455
  • Compressive Strength, ISO.899 DIN.53444, 1% strain over 1000 hours
  • Charpy Impact Unnotched, ISO.R179 DIN.53453, 7.5 J
  • Charpy Impact, Notched, ISO179/3C DIN.53453
  • Coefficient of Friction, Dynamic, on dry ground steel; load =0.05MPa; speed =0.6 m/s
  • Volume Resistivity, ISO.93 DIN.53482
  • Dielectric Constant, ISO.250 DIN.53483
  • Dielectric Strength, ISO.243 DIN.53481
  • Dissipation Factor, ISO.250 DIN.53483
  • CTE, linear
  • Thermal Conductivity, DIN.52612
  • Maximum Service Temperature, Air, Continuous; 5000 hours based on a tensile stress of 50% at 23° C.
  • Maximum Service Temperature, Air, short period, no load
  • Deflection Temperature at 1.8 MPa (264 psi), ISO.75 DIN.53461
  • Minimum Service Temperature, Air, impact conditions and heavy loads not considered
  • Flammability, UL94
  • Flammability, UL94
  • Oxygen Index, ISO.4589
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Omnia Plastica s.p.a.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.