MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Sandvik Bioline 1RK91 Precision Wire
Categories: Metal; Ferrous Metal; Ferritic; Stainless Steel; Precipitation Hardening Stainless

Material Notes: Sandvik Bioline 1RK91 (a Sandvik NanoflexTM material) is a precipitation hardening stainless steel grade specifically designed for applications requiring high strength combined with good ductility in the final product and high formability in the as-delivered condition. The strength is increased after ageing of the final product.

The characteristics in general can be said to be a combination of properties of ordinary austenitic stainless and low alloyed ferritic steels. This means that properties such as elastic modulus, mechanical properties and thermal expansion are comparable to ferritic steels (such as low alloyed carbon steels or chromium steels) while properties such as corrosion resistance is more comparable to austenitic stainless steels.

  • excellent mechanical properties, very high tensile strength and hardness levels can be achieved
  • corrosion resistance comparable to AISI 304L or AISI 316L depending on condition
  • retained mechanical properties at temperatures up to at least 400oC good weldability
  • Information provided by Sandvik

    Vendors:
    Available Properties
    • Density
    • Tensile Strength
    • Tensile Strength
    • Tensile Strength
    • Tensile Strength
    • Tensile Strength
    • Tensile Strength
    • Tensile Strength
    • Tensile Strength
    • Tensile Strength
    • Tensile Strength
    • Tensile Strength, Ultimate, Annealed, Strip
    • Tensile Strength, Ultimate, Cold rolled, Strip
    • Tensile Strength, Ultimate, Cold Worked, flat rolled
    • Tensile Strength, Ultimate, Cold Worked, round
    • Tensile Strength, Ultimate, aged, bar
    • Tensile Strength, Ultimate, Aged, flat rolled
    • Tensile Strength, Ultimate, Cold rolled + aged, Strip
    • Tensile Strength, Ultimate, Aged, round
    • Tensile Strength, Ultimate, 475-530°C for 4 hours, Bar form
    • Tensile Strength, Ultimate, 475-530°C for 4 hours, Bar form
    • Tensile Strength, Ultimate, 475-530°C for 4 hours, Bar form
    • Tensile Strength, Ultimate, 475-530°C for 4 hours, Bar form
    • Tensile Strength, Ultimate, 475-530°C for 4 hours, Wire and strip form
    • Tensile Strength, Ultimate, 475-530°C for 4 hours, Bar form
    • Tensile Strength, Ultimate, 475-530°C for 4 hours, Wire and strip form
    • Tensile Strength, Ultimate, 475-530°C for 4 hours, Wire and strip form
    • Tensile Strength, Ultimate, 475-530°C for 4 hours, Wire and strip form
    • Tensile Strength, Ultimate, 475-530°C for 4 hours, Wire and strip form
    • Tensile Strength, Yield, Annealed, Strip
    • Tensile Strength, Yield, Cold worked, Bar
    • Tensile Strength, Yield, Cold rolled, Strip
    • Tensile Strength, Yield, Cold Worked, flat rolled
    • Tensile Strength, Yield, Aged, Bar
    • Tensile Strength, Yield, Aged, flat rolled
    • Tensile Strength, Yield, Cold rolled + aged, Strip
    • Modulus of Elasticity, Tensile Strength-1000 MPa
    • Modulus of Elasticity, Tensile Strength-1850 MPa
    • CTE, linear, Cold worked
    • CTE, linear, Cold worked
    • CTE, linear, Cold worked
    • CTE, linear, Cold worked
    • CTE, linear, Cold worked
    • CTE, linear, Aged
    • CTE, linear, Aged
    • CTE, linear, Aged
    • CTE, linear, Aged
    • Specific Heat Capacity
    • Specific Heat Capacity
    • Specific Heat Capacity
    • Specific Heat Capacity
    • Specific Heat Capacity
    • Thermal Conductivity
    • Thermal Conductivity
    • Thermal Conductivity
    • Thermal Conductivity
    • Thermal Conductivity
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    none

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Aluminum Castings
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.