Advanced Performance Terpolymer (APT) produced using Exxon Chemical's EXXPOL technology. Specifically designed for monolayer blown film applications and has an outstanding balance of end-use performance (toughness, opticals, sealability, hot tack) and processability.
Applications: Tough monolayer blown films, laminations films and special sealant films. Data for film properties below based on 1.25 mil film.
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticThermoplastic Elastomer