MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond Supreme 3HTND-2GT One Part, Toughened, Fast Curing Glob Top Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Excellent thermal conductivity
  • Fast curing
  • Withstands thermal cycling and shock
  • Serviceable from 100°F to +400°F
Product Description: Master Bond Supreme 3HTND 2GT is a fast curing, toughened multifunctional one component high performance epoxy system that can be used for bonding, sealing, glob top and die attach applications. It has a huge array of highly desirable features, including no mixing, a convenient viscosity, sterling physical properties and very fast cures. Unlike many epoxies it can be readily and efficiently applied to a defined area. This epoxy combines excellent electrical insulation properties and thermal conductivity with top-notch dimensional stability and the capability of withstanding rigorous thermal cycling and shocks. It cures in 20-30 minutes at 250°F or in 5-10 minutes at 300°F with very low shrinkage. Supreme 3HTND-2GT can cure in thicknesses of up to 1/8 inch if needed. It bonds well to a wide variety of substrates used in electronics, including metals, composites, ceramics and many plastics. The service temperature range for this system is first rate at -100°F to +400°F. It resists chemicals rather well, including water, acids, bases and many solvents. Especially noteworthy, is its low level of ionic impurities. Supreme 3HTND-2GT is yellowish tan in color. As mentioned above, this multifaceted system can be used as a glob top or die attach and in other applications as an adhesive or sealant in electronics when the special combination of properties, particularly the limited flow characteristics when curing are desirable.

Product Advantages:

  • Single component system; no mixing needed prior to use
  • Convenient handling; ideal flow for die attach and glob top applications
  • 100% reactive, no volatiles emitted during cure
  • Outstanding electrical insulation properties and thermal conductivity
  • Excellent physical strength properties
  • Sterling dimensional stability
  • Service temperature range of -100°F to +400°F
  • Offers exquisite protection to electronic components
  • Available and easily dispensed from syringes

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Solids Content
  • Hardness, Shore D
  • Tensile Strength
  • Tensile Modulus
  • Compressive Strength
  • Adhesive Bond Strength, Tensile Lap, Aluminum to Aluminum
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Cure Time
  • Cure Time
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.