MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
KaMin KaMin® 90B Kaolin Clay - Waterwashed
Categories: Ceramic; Clay; Kaolin Clay

Material Notes: KaMin® 90B is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90B is ideally suited for water-borne applications where high gloss, holdout and controlled rheology are important.

Industry: Paint & Coatings, Adhesives & Sealants, Ink

Uses: Architectural Coatings, Industrial Coatings, Flat/Matte, Satin, Primer, Water Based, Gravure Water Based, Flexo Water Based

Information provided by KaMin LLC.

Vendors:
Available Properties
  • Specific Gravity
  • Bulk Density, Loose
  • Solids Content, Slurry
  • Brightness, Reflectance (TAPPI)
  • Oil Absorption
  • Fineness, Hegman Grind
  • Moisture Absorption at Equilibrium, As Produced
  • Particle Size, Average Stokes Equivalent Diameter
  • Particle Size, Median (Malvern Laser)
  • Particle Mesh Size, 0.005% Retained
  • pH, 100 g/250 ml H2O Slurry
  • Specific Surface Area, BET
  • Brookfield Viscosity, 20 RPM
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.