MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.08 psf)
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported versions contain a woven nylon carrier for glueline thickness control and improved handleability. Redux 319 is a hot melt film which is free from solvents and consequently it has a very low volatile content.

Features: Cures in 60 min at 350°F; Good performance at temperatures ranging from -67°F to 300°F; Good short-term exposure performance at 350°F; Excellent peel properties; Good drape at ambient temperatures; Less than 1% volatile content.
Applications: Aluminum to aluminum bonding; Fiber-reinforced composite to composite bonding; Aluminum honeycomb sandwich bonding; Aramid honeycomb sandwich bonding.

Vendors:
Available Properties
  • Tensile Strength, Yield, Flatwise Tensile
  • Tensile Strength, Yield, Flatwise Tensile, Primed with Redux 119
  • Shear Strength, Lap Shear Unprimed, 12 months at 300°F
  • Shear Strength, Lap Shear Unprimed, 12 months at 300°F
  • Shear Strength, Lap Shear
  • Shear Strength, Lap Shear Unprimed, No conditioning of Redux 319
  • Shear Strength, Lap Shear Primed, No conditioning of Redux 319
  • Shear Strength, Lap Shear, Primed with Redux 119
  • Shear Strength, Lap Shear Unprimed, 1000 hrs in water/methanol at 72°F
  • Shear Strength, Lap Shear Unprimed, 1000 hrs in Skydrol 500A at 72°F
  • Shear Strength, Lap Shear Unprimed, 1000 hrs in distilled water at 72°F
  • Shear Strength, Lap Shear Unprimed, 1000 hrs in Silcodyne 'H' at 72°F
  • Shear Strength, Lap Shear Primed, 1000 hrs in distilled water at 72°F
  • Shear Strength, Lap Shear Primed, 1000 hrs in water/methanol at 72°F
  • Shear Strength, Lap Shear Unprimed, 1000 hrs in hydraulic oil at 72°F
  • Shear Strength, Lap Shear Primed, 1000 hrs in Skydrol 500A at 72°F
  • Shear Strength, Lap Shear Unprimed, No conditioning of Redux 319
  • Shear Strength, Lap Shear Unprimed, 1000 hrs in synthetic esters at 72°F
  • Shear Strength, Lap Shear Primed, 1000 hrs in synthetic esters at 72°F
  • Shear Strength, Lap Shear Unprimed, 1000 hrs in anti-icing fluid at 72°F
  • Shear Strength, Lap Shear Unprimed, 1000 hrs in Kerosene fuel at 72°F
  • Shear Strength, Lap Shear Primed, 1000 hrs in Kerosene fuel at 72°F
  • Shear Strength, Lap Shear Primed, No conditioning of Redux 319
  • Shear Strength, Lap Shear Primed, 1000 hrs in Silcodyne 'H' at 72°F
  • Shear Strength, Lap Shear Primed, 1000 hrs in anti-icing fluid at 72°F
  • Shear Strength, Lap Shear Primed, 1000 hrs in hydraulic oil at 72°F
  • Peel Strength, Bell Peel
  • Peel Strength, Bell Peel, Primed with Redux 119
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.