MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Global EPP PA 6C Cast Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of cast nylons may be altered to suit specific applications, and the performance of the basic polymer can be enhanced with the addition of various additives, fillers, lubricants and colorants.

Key characteristics:

  • Unequalled formulation options and profile range
  • Excellent mechanical, thermal and chemical resistance
  • Excellent PV and load bearing capabilities
  • Excellent wear and abrasion resistance
  • Good dimensional stability, largely free from internal stresses
  • FDA compliant grades available

This unmodified grade, produced by an anionic polymerisation casting process, demonstrates similar characteristics to PA 66 E. Cast products contain significantly lower stress levels combined with high strength, good creep and wear resistance resulting in great dimensional accuracy when machining.

Vendors:
Available Properties
  • Density, ISO 1183:1987, Test Method A
  • Water Absorption, ISO 62:1999 (modified), Immersion
  • Water Absorption at Saturation, ISO 62:1999
  • Hardness, Shore D, ISO 868:2003
  • Tensile Strength at Break, ISO 527-1/2:1993, Sample Type 1B, 50mm/min
  • Elongation at Break, ISO 527-1/2:1993, Sample Type 1B, 50 mm/min
  • Modulus of Elasticity, ISO 527-1/2:1993, Sample Type 1B, 50 mm/min
  • Flexural Strength, ISO 178:2001, 1.5 mm/min
  • Flexural Modulus, ISO 178:2001, 1.5 mm/min
  • Compressive Strength, ISO 604:2002, Sample Type B, 5 mm/min
  • Compressive Modulus, ISO 604:2002, Sample Type A, 1 mm/min
  • Izod Impact, Notched (ISO), ISO 180:2000, Sample Type A
  • Coefficient of Friction, Dynamic, 31.4 m/min
  • K (wear) Factor, 31.4 m/min
  • Volume Resistivity, IEC 60093:1980-01
  • Surface Resistance, IEC 60093:1980-01
  • Dielectric Constant, IEC 60250:1969-01
  • Dielectric Constant, IEC 60250:1969-01
  • Dielectric Strength, IEC 60243-1:1998-01
  • Comparative Tracking Index, IEC 60112:2003-01
  • CTE, linear, ISO 11359-2:1999
  • Thermal Conductivity, ISO 8301:1991
  • Melting Point
  • Maximum Service Temperature, Air, Continuous
  • Maximum Service Temperature, Air, Intermittent
  • Minimum Service Temperature, Air, Intermittent
  • Minimum Service Temperature, Air, Continuous
  • Flammability, UL94, IEC 60695-11-10:2003-08
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.