MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phillips 66 Tropa Artic® Synthetic Blend Motor Oil SAE Grade 0W-20
Categories: Fluid; Lubricant

Material Notes: Phillips 66® TropArtic Synthetic Blend Motor Oil is a premium quality, part-synthetic automotive engine oil designed to provide excellent engine protection for gasoline-fueled and flex-fuel passenger cars and light trucks under all operating conditions. TropArtic Synthetic Blend Motor Oil is formulated to provide excellent wear protection, to minimize sludge and varnish formation, and to resist viscosity and thermal breakdown, even in severe service. It also protects against rust and bearing corrosion, and is resistant to foaming. The part-synthetic formulation provides enhanced oxidation resistance and thermal stability at high temperatures and better pumpability at low temperatures compared with conventional engine oils, for extra protection under all driving conditions. TropArtic Synthetic Blend Motor Oil exceeds new car warranty requirements as defined by ILSAC GF-5. It meets “Resource Conserving” requirements for fuel economy improvement, emission system and turbocharger protection, and protection of engines operating on ethanol-containing fuels up to E85. It is backward serviceable for use where API SM or earlier “S” category engine oils are recommended.

Applications:

  • Gasoline-fueled and flex-fuel passenger cars, light trucks and sport utility vehicles, including gasoline-electric hybrids
  • Four-stroke gasoline engines in other mobile or stationary equipment
TropArtic Synthetic Blend Motor Oil is licensed for:
  • ILSAC GF-5
  • API Service SN with Resource Conserving
TropArtic Synthetic Blend Motor Oil meets or exceeds the requirements of:
  • Chrysler MS-6395 (Rev. T) (SAE 5W-20, 5W-30, 10W-30)
  • Ford WSS-M2C945-A (SAE 5W-20), WSS-M2C946-A (SAE 5W-30)
  • GM6094M (obsolete specification)
Features/Benefits:
  • Exceeds ILSAC GF-5 requirements for new cars under warranty
  • Friction-modified for improved fuel economy
  • Excellent resistance to viscosity and thermal breakdown at high temperatures
  • Protects against sludge and varnish formation
  • Protects against wear and bearing corrosion
  • Low volatility for reduced oil consumption
  • Excellent low-temperature pumpability for protection during cold starts
  • Highly resistant to foaming
  • Formulated to protect turbochargers and emissions control system catalysts
  • Formulated for use in vehicles operating on ethanol-containing fuels up to E85

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Viscosity, High-Temp/High-Shear
  • Viscosity, Cold Cranking
  • Viscosity Measurement, Index
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Ash, ASTM D874, Sulfated
  • ASTM Color, ASTM D1500
  • Total Base Number, ASTM D2896
  • Pour Point
  • Flash Point, COC
  • Phosphorus, P
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.