| Chemical recycled PET (Recycle content 25%); Excellent processability, high transparency, Excellent thermal stability, recyclability and reusability Applications: Soft drink and mineral water container, transparent sheets, packaging materials, other extrusion and injection products Information provided by Lotte Advanced Materials. |