MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Chemours Viton® B-202 with 5 phr N990 Carbon Black
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Viton® B-202 is a low viscosity, B-type gum polymer that demonstrates improved processing and rheology when compared with existing fluoroelastomers. Viton® B-202 is designed to be cured with either Viton® Curative #30 or Viton® Curative #50. When using Viton® Curative #30, use Viton® Curative #20 in a ratio of about 1.8 Viton® Curative #30 to Viton® Curative #20. When using Viton® Curative #50, use 0.3–0.5 phr of Viton® Curative #20 to ensure a fast cure rate. Note that Viton® Curative #20 can be difficult to mix into low viscosity stocks, such as those based on Viton® B-202, and careful attention needs to be paid to mixing procedures. Compared with other B-family terpolymers, Viton® B-202 provides:
  • Low viscosity
  • Improved processing
  • Increased mold flow
  • Excellent mold release

Applications:

  • Transfer and injection molding of complex shapes
  • Extrusions (e.g., fuel hose and tubing)
  • Solution coatings of fabrics, tanks or chemical containers

Viton® B-202 can be blended with other Viton® types to modify viscosity, enhance processability and/or improve flow.

Information provided by manufacturer.

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors:
Available Properties
  • Mooney Viscosity, ML 1 + 10
  • Hardness, Shore A, Cured 10 min at 177°C and Post Cured 24 hr at 232°C
  • Tensile Strength, Ultimate, Cured 10 min at 177°C and Post Cured 24 hr at 232°C
  • Elongation at Break, Cured 10 min at 177°C and Post Cured 24 hr at 232°C
  • 100% Modulus, Cured 10 min at 177°C and Post Cured 24 hr at 232°C
  • Compression Set, Method B, Plied Disks, 70 hr
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chemours, former DuPont

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.