| KEBAFORM C904 UR is a normal viscosity, elastomer-containing injection molding grade based on KEBAFORM C 90.0. The increased elastomer content results in a very high toughness level. The absorption capacity for high dynamic loads is excellent. Fields of application include outset technology, track rollers, belt buckles, transport chains, fastening elements, etc. Properties: dimensionally stable, good chemical resistance, good gliding properties, good recovery behavior, impact resistant, semi-crystalline Typical areas of application: Gears, Fasteners, Spring elements, Handles, Belt buckles, industrial goods, Bearing bushes, Outset technology, Pneumatic tubes, Rollers, Sports & Leisure Articles, shockproof housing, Transport chains, Valves, Connecting elements Information provided by BARLOG plastics GmbH. |