| PPS-GF40, linear PPS, 40% glass fiber reinforced, hydrolysis stabilized Properties: dimensionally stable, good aging behavior, good fire behavior, high continuous used temperature, High strength, hydrolysis stable, semi-crystalline Typical areas of application: Housing, Lamp socket, Pump housing, Sensors, Bobbin, Plug, Valve caps, Distributor Industries: Automotive, Electrical and electronics industry, Household appliances, Aviation Industry, Mechanical Engineering Information provided by BARLOG plastics GmbH. |