MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
CeramTec Rubalit® A 1999.5 Alumina, 99.7%
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon materials is especially suitable for plain bearings and seal rings.

Key Words: Al2O3, aluminum oxide
Vendors:
Available Properties
  • Density, DIN EN 623-2 / ASTM-C373 / ASTM-C20
  • Water Absorption, DIN EN 623-2 / ASTM-C373
  • Permeability, Gas
  • Weibull Modulus, DINV ENV 843-5
  • Vickers Microhardness, DINV ENV 843-4, HV 0.5
  • Tensile Strength at Break, ACMA Test #4 / DIN EN 843-1
  • Tensile Modulus, DINV ENV 843-2 / ASTM-F417, Young's
  • Flexural Strength, DIN EN 843-1
  • Flexural Strength, ASTM-F417, Bending Strength; 4-Point Method (40x4x3 mm³)
  • Compressive Strength, ASTM C-773-88 / DIN 51067T1
  • Poissons Ratio, DINV ENV 843-2
  • Fracture Toughness, DIN 51109
  • Shear Modulus, Calculated
  • Volume Resistivity, IEC 672-1
  • Volume Resistivity, IEC 672-1
  • Volume Resistivity, IEC 672-1
  • Dielectric Constant, IEC 672-1 / ASTM-C150
  • Dielectric Strength, 6.35 mm (1/4") IEC 672-1
  • Dielectric Loss Index, IEC 672-1 / ASTM-D149,150
  • CTE, linear, DIN EN 821-1
  • CTE, linear, DIN EN 821-1
  • CTE, linear, DIN EN 821-1
  • CTE, linear, DIN EN 821-1
  • Specific Heat Capacity, DINV ENV 821-3
  • Thermal Conductivity, DIN EN 821-2 / ASTM-C408
  • Maximum Service Temperature, Air
  • Maximum Service Temperature, Inert
  • Al2O3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
CeramTec North America

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.