MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Dalau Dalcon 001 100% Virgin PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Applications & Industries:
General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.
Chemical: Dynamic & shaft seals; Pipes & tubing for carrying chemicals; and Seals & gaskets. Flat gaskets are used to seal flanges in pipelines.
Construction: Bridge bearings. Slide bearings.
Electrical: Communications, radio & television engineering, cable insulation; Electrical plant construction & electronics industry (connectors & terminals); General electrical equipment (P.T.F.E. excellent electrical insulating material); and Power plant installations (switchgear).
Engineering: Anti - friction bearing cages & bearing plates; Bearings and bushes; Diaphragm pumps. Film bearings. Multi - layer composite bearings. Fabric bearings; Laboratory equipment. Measuring & control technology; Pipe supports. Expansion bellows. Glandless valves & pumps, valve seats; Piston rings in hydraulic systems; and Piston rod packings used in compressor plunger pumps & valves.
Food: Dynamic & shaft seals (used in the food processing industry) and Linings & coatings (fertiliser plant & food industry line equipment).

CHEMICAL RESISTANCE: The strength of the carbon - fluorine bond and the shielding of the carbon chains by the fluorine atoms result in a chemical inertness which is virtually universal, except alkali metals, fluorine under certain conditions, and some fluorine compounds at elevated temperatures. Some Fluorinated Hydrocarbons (refrigerants) cause reversible swelling i.e. Tetrafluorodichloroethane Frigen 21, giving a 9.6% weight increase. For specific data on chemical resistance of this material we have a computer database with all the information covering over 90% of all known chemicals.

Information provided by Dalau

Vendors:
Available Properties
  • Density, BS2782:Pt6
  • Deformation, ASTM D621, Permanent Deformation
  • Deformation, ASTM D621, 150°C
  • Deformation, ASTM D621
  • Deformation, ASTM D621
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, BS2782:Pt3, Molding Direction
  • Elongation at Break, BS2782:Pt3, Molding Direction
  • Flexural Modulus, ASTM D790
  • Compressive Modulus, ASTM D621
  • Coefficient of Friction, Dynamic, ASTM D1894
  • Coefficient of Friction, Static, ASTM D1894
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149, Oil(Molding)
  • Dielectric Strength, ASTM D149, Oil (Extrusion)
  • Dielectric Strength, ASTM D149, Air (Tape)
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • CTE, linear, Parallel to Flow, ASTM D696
  • CTE, linear, Transverse to Flow, ASTM D696
  • Thermal Conductivity, ASTM C177, Molding Direction
  • Melting Point, ASTM D3417
  • Maximum Service Temperature, Air
  • Maximum Service Temperature, Air, Short Periods
  • Minimum Service Temperature, Air
  • Flash Point, ASTM D1929
  • Oxygen Index, ASTM D2863
  • Haze, ASTM D1003
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.