MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Borealis Borcoat" BB127E-PW Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Borcoat BB127E-PW is a maleic anhydride grafted polypropylene (PP) adhesive. The product is non-pigmented (not colored) and available in powder form for spray application.

Applications: Steel pipe coating Borcoat BB127E-PW is intended to be used as an adhesive in three-layer-PP based anti-corrosion or in multi-layer-PP based thermal insulation coatings at design temperatures up to 110°C for onshore and 140°C for offshore applications. Borcoat BB127E-PW is intended to fulfill below mentioned national and international standards and specifications, when appropriate industrial manufacturing standard procedures are applied, a continuous quality system is implemented and when used in combination with a compatible Fusion Bonded Epoxy (FBE) powder and the top-coat material Borcoat BB108E-1199.

Specifications: Borcoat BB127E-PW and/or articles produced from it, are expected to meet the applicable requirements included in the below mentioned standards provided it is processed using sound material handling and processing practices as well as appropriate testing procedures. DIN 30678 EN ISO 21809-1; DNVGL-RP-F106; NF A49-711

Information provided by Borealis AG

Vendors:
Available Properties
  • Density, ISO 1183-1/Method A
  • Particle Size, ASTM D1921, 0-25%
  • Particle Size, ASTM D1921, 55-85%
  • Particle Size, ASTM D1921, 0-25%
  • Particle Size, ASTM D1921, 0-20%
  • Melt Flow, ISO 1133-1
  • Tensile Strength, Yield, ISO 527-2, 50 mm/min
  • Elongation at Yield, ISO 527-2, 50 mm/min
  • Tensile Modulus, ISO 527-2, 1 mm/min
  • Flexural Modulus, ISO 178, 2 mm/min
  • Charpy Impact, Notched, ISO 179-1/1eA
  • Peel Strength, ISO 21809-1, 3 layer
  • Peel Strength, ISO 21809-1, 3 layer
  • Peel Strength, ISO 21809-1, 3 layer
  • Peel Strength, ISO 21809-1, 3 layer
  • Melting Point, ISO 11357-3
  • Vicat Softening Point, ISO 306, A50
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.