MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SEKISUI SPI KYDEX® FST Thermoplastic sheet
Categories: Polymer; Thermoplastic

Material Notes: KYDEX® FST is a proprietary, high performance thermoplastic sheet formulated to meet all Boeing and Airbus toxicity requirements for aircraft interior components.

KYDEX® FST meets all flame, smoke, and heat release requirements set forth in Federal Aviation Regulations (FAR) 25.853 paragraphs (a) and (d) as well as toxicity requirements for Airbus (ABD003) and Boeing (BSS7239). Its excellent properties make it the ideal material to form two and three-dimensional aircraft components.

Suggested Application:

  • Seat parts
  • Bulkhead laminates
  • Life vest shrouds
  • Passenger service units
  • Monitor Shrouds
  • Armrests
  • Molding strips
  • Tray tables
  • Kick panels
Features:
  • Meets the stringent requirements of FAR 25.853 (a) and (d) in all thicknesses and colors
  • Meets toxicity smoke requirements of Airbus (ABD0031) and Boeing (BSS7239)
  • Excellent fabrication and formability characteristics
  • Allows for tight tolerance control
  • Available in a wide range of integral colors

Information provided by SEKISUI KYDEX, LLC.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Yield Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Bearing Yield Strength, ASTM D953
  • Bearing Yield Strength, ASTM D953
  • Poissons Ratio, ASTM D638
  • Shear Strength, ASTM D732
  • Gardner Impact, ASTM D5420, Drop Dart Impact, GE
  • Dielectric Strength, ASTM D149, oil
  • CTE, linear, ASTM E831
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, annealed
  • Smoke Density, FAR 25.853(d) Part V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.