MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Evonik Paraglas Soundstop® Transparent Sheet  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Sheet

Material Notes: Paraglas Soundstop is a standard clear transparent sheet

Information provided by Cyro Industries

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors:
Available Properties
  • Density, ASTM D792
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Charpy Impact Unnotched, ASTM D4812, Weathered 5 years
  • Charpy Impact Unnotched, ASTM D4812, At -5°F
  • Charpy Impact Unnotched, ASTM D4812
  • Sound Insulation, ASTM E 90
  • Sound Insulation, ASTM E 90
  • Sound Insulation, ASTM E 90
  • CTE, linear, ASTM D696
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Vicat Softening Point, ASTM D1525
  • Flame Spread, ASTM D635
  • Smoke Density, ASTM D2843, percent
  • Ignition Temperature, ASTM D1929, Self Ignition
  • Refractive Index, ASTM D542
  • Haze, ASTM D1003
  • Haze, ASTM D1003, Weathered 5 years AZ
  • Yellow Index, ASTM E 313
  • Yellow Index, ASTM E 313, Weathered 5 years AZ
  • Transmission, Visible, Weathered 5 years AZ
  • Transmission, Visible, ASTM D1003
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.