| SSAB Docol 460LA is available both as hot rolled and cold rolled. SSAB Docol HR460LA-UC can after agreement be adapted and delivered as dual certified with S460MC according to EN 10149-2. Dimension Range: Cold rolled / UC: thickness 0.50-2.10 mm, width up to 1527 mm. Cold rolled / GI, GA, ZA: thickness 0.80-2.00 mm, width up to 1410 mm. Hot rolled / UC: thickness 2.00-6.00 mm, width up to 1600 mm. Slit strip and cut to length sheets are available upon request. Grade and coating specific restrictions on available dimensions may occur. Data provided by SSAB. |