MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Polynt POLYCOR® 945XJ142UP Vinyl Ester Tooling Gel Coat
Categories: Polymer; Thermoset

Material Notes: Vinyl Ester Tooling Gel Coats are specifically formulated with selected vinyl ester resins that exhibit high Heat Distortion Temperature to withstand the repeated molding of FRP laminates. They provide a high gloss and hard durable surface. These tooling gel coats are ready to be sprayed after the addition of the proper amount of the appropriate of promoters, then the right amount of methyl ethyl ketone peroxide. Read application instructions carefully, because even though manufacturing precautions are used to make tooling gel coat, a misapplication of these products can produce unacceptable results.

Information provided by Polynt Composites.

Vendors:
Available Properties
  • Volatile Organic Compounds (VOC) Content
  • Brookfield Viscosity, RVT, Spindle No.5 @ 20 rpm
  • Flash Point
  • Cure Time, Lay-up Time
  • Gel Time, Reactivity at 25°C, using 2.0% of MEKP-925
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.