MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik VESTAMID® LX9042 NC Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® LX9042 NC is an easy mold release and heat stabilized compound. Due to its highly effective mold release agents, VESTAMID® LX9042 NC is suitable for the efficient production of injection molded parts with very short cycle times. In addition, VESTAMID® LX9042 NC is nucleated to reduce the cycle time even further and/or to reduce the shrinkage. Properties of compounds based on Polyamide12 vary little with changing humidity due to their low moisture absorption. Parts made of this semicrystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance. VESTAMID® LX9042 NC is supplied as cylindrical granules, ready for processing, in moisture-proof bags. Pigmentation may affect values.
Dry properties listed below
Industrial Sector: Sustainable, Industry and Engineering
Sustainability: Sustainable electricity
Processing: Injection molding
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability)
Additives: Release agent, Unfilled
Special Characteristics: High heat resistant, Medium viscosity, Low warpage / Low shrinkage
Features: Low coefficient of friction, Nucleated
Color: Natural color
Additives: Release agent
Chemical Resistance: General chemical resistance

Information provided by Evonik.

Vendors:
Available Properties
  • Water Absorption, Sim to ISO 62
  • Viscosity Number, ISO 307, 1157, 1628
  • Linear Mold Shrinkage, Flow, ISO 294-4, 2577
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 2577
  • Melt Flow, ISO 1133
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, ISO 527
  • Tensile Stress, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527, Nominal
  • Elongation at Yield, ISO 527
  • Tensile Modulus, ISO 527
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Melting Point, ISO 11357-1/-3
  • Vicat Softening Point, ISO 306, 50 K/h
  • Vicat Softening Point, ISO 306, 50 K/h
  • Melt Temperature
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.