| NTG-10 is one of our polyurethane gel formulations to make a soft elastomeric material with a good cushioning effect, better strength, and a less tacky surface compared to the commonly available polyurethane gel formulations. NTG-10 may be suited to make shoe insoles, handle grips, and many other custom products. The low viscosity values of the component materials allow easy handling and replication of an intricate mold surface design. The standard catalyst package allows a long pot life for ease of the process. The curing rate can be sped up by catalyst(s). NTG-10 does not bottom out from compression as readily as foams. This formulation can be used in cushioning/padding products supplementing foam to support pressure points. NTG-10 can also simulate many TPE (thermoplastic elastomer) class polymer parts. Whereas TPE polymers require high heat and high-pressure injection molding processes, NTG-10 can be processed at room temperature* in ambient pressure molds. NTG-10 may be an ideal material for prototyping or simulating TPE parts. (Note*: Although it can sure at room temperature, mold temperature of 120 – 190 °F is recommended for a less tacky surface.) Mixing Ratio: 21: 100 = Part-A: Part-B by Volume Ratio 100: 449 = Part-A: Part-B Weight Ratio Designations: System Code: NTG-10 Part-A: MPB-028 Part-B: PPB-131 Information provided by Northstar Polymers |