MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond Supreme 34CA Two component epoxy system
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes:
  • Very high temperature resistance
  • Robust resistance to aggressive chemicals
  • Very long open time
  • Good flow properties
Master Bond Supreme 34CA is a two component epoxy system specially formulated to resist higher temperatures and aggressive chemicals. This lower viscosity material has an easy to use 100 to 50 mix ratio by weight. It will not cure at room temperature and it has an exceptionally long working life, far exceeding 24 hours. Although, it is slightly exothermic, it can be cured in sections exceeding 1/4 inch thick. Particular attention should be paid to the curing schedule. The main attribute of Supreme 34CA is as a high temperature resistant structural type adhesive, although it has many other outstanding properties as well. In this context, it can be used for filament winding, tooling compounds along with bonding composites and pultruded structures. As mentioned previously, it bonds well to a wide variety of substrates, including metals, composites, glass and many plastics. Supreme 34CA is highly resistant to water, oils, acids, bases and solvents. It has top notch physical strength properties and is a superior electrical insulator. The color of Part A is black, and Part B is amber. The service temperature range for this system is -80°F to +500°F. A non-drip version is available, called Supreme 34CAND-2. Supreme 34CA is specified in many applications in aerospace, electronics, optical and specialty OEM uses.

Product Advantages:

  • Lower viscosity; very long open time
  • Superb adhesion to a wide variety of substrates
  • Ample physical strength properties
  • Terrific resistance to aggressive chemicals especially acids, bases and petroleum related
  • Commanding high temperature serviceability
  • Excellent compatibility with filament winding and bonding composites

Information provided by Masterbond.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, mixed
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength
  • Tensile Modulus
  • Adhesive Bond Strength, lap shear, Al/Al
  • Volume Resistivity
  • Dielectric Constant
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Working Life, After mixing, 100 g batch
  • Shelf Life, In original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.