MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
BASF Ultramid® 8202 PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ultramid 8202 HS) and/or pigmented versions. It combines good strength, stiffness and toughness as well as excellent heat, chemical and abrasion resistance.

Vendors:
Available Properties
  • Density, ISO 1183
  • Melt Density, ISO 1183
  • Water Absorption, ISO Test, 24 hour
  • Water Absorption, ISO 62
  • Moisture Absorption at Equilibrium, ISO 62, 23°C/50% R.H.
  • Relative Viscosity, ISO Test; 96 % SAV
  • Viscosity Measurement, Formic Acid
  • Linear Mold Shrinkage, ASTM Data; MD
  • Hardness, Rockwell R, ASTM Test
  • Tensile Strength at Break, ASTM Test, 0.2 in/min
  • Tensile Strength, Yield, ISO 527, 50mm/min
  • Tensile Strength, Yield, ASTM Test, 2 in/min
  • Tensile Strength, Yield, ISO Data
  • Tensile Strength, Yield, ASTM Test
  • Tensile Strength, Yield, ASTM Test
  • Tensile Strength, Yield, ISO Data
  • Tensile Strength, Yield, ASTM Test
  • Tensile Strength, Yield, ISO Data
  • Elongation at Break, ISO 527, 50mm/min, Nominal strain
  • Elongation at Break, ASTM Test, 2 in/min
  • Elongation at Yield, ISO 527, 50mm/min
  • Elongation at Yield, ASTM Test, 2 in/min
  • Elongation at Yield, ISO Data
  • Elongation at Yield, ASTM Test
  • Elongation at Yield, ISO Data
  • Elongation at Yield, ASTM Test
  • Tensile Modulus, ISO 527, 1mm/min
  • Tensile Modulus, ISO Data
  • Tensile Modulus, ISO Data
  • Flexural Strength, ISO Data
  • Flexural Strength, ASTM Test
  • Flexural Strength, ASTM Test
  • Flexural Strength, ASTM Test
  • Flexural Strength, ASTM Test
  • Flexural Strength, ASTM Test
  • Flexural Modulus, ISO Data
  • Flexural Modulus, ASTM Test
  • Flexural Modulus, ASTM Test
  • Flexural Modulus, ASTM Test
  • Flexural Modulus, ASTM Test
  • Izod Impact, Notched, ASTM Test
  • Izod Impact, Notched, ASTM Test
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Volume Resistivity, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, ASTM Data
  • Dielectric Constant, ASTM Data
  • Dielectric Strength, IEC 60243-1
  • Dissipation Factor, ASTM Data
  • Dissipation Factor, ASTM Data
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, IEC 60112
  • CTE, linear, ASTM Test
  • Specific Heat Capacity, Melt
  • Thermal Conductivity, Melt
  • Melting Point, 10 K/min
  • Melting Point, ASTM Test
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM Test
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM Test
  • Flammability, UL94
  • Flammability, UL94
  • Melt Temperature, Injection molding
  • Mold Temperature, Injection molding
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.