MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik VESTAKEEP® 50001XT BK PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: VESTAKEEP® 50001XT BK is a high viscosity, unreinforced, unlubricated polyether ether ketone for injection molding and extrusion and can be cross-linked after processing by heat treatment. The semi-crystalline polymer features superior property retention at elevated temperatures combined with the chemical resistance of standard PEEK. Parts made from VESTAKEEP® 50001XT BK feature a very high resistance to creep. VESTAKEEP® 50001XT BK can be processed by common machines for PEEK processing. VESTAKEEP® 50001XT BK is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners. As VESTAKEEP® 50001XT BK is a reactive system the manufacturer recommends low melt temperatures and short cycle times. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C. Preliminary data sheet.
Dry properties listed below
Industrial Sector: Energy, Oil and Gas
Processing: Injection molding
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), Fire / burn
Special Characteristics: Semi-crystalline, Crosslinkable, High viscosity
Features: Creep resistance, Low coefficient of friction
Color: Black

Information provided by Evonik.

Vendors:
Available Properties
  • Density, ISO 1183
  • Melt Flow, ISO 1133
  • Hardness, Shore D, ASTM D2240, annealed
  • Coefficient of Friction, ISO 7148-2
  • K (wear) Factor, ISO 7148-2, parallel, Test speed: 0.5 m/s
  • Melting Point, ASTM D3418
  • Glass Transition Temp, Tg, ISO 11357-1/-2
  • Melt Temperature, ISO 294, Injection Molding
  • Mold Temperature, ISO 294, Injection Molding
  • Injection Velocity, ISO 294, Injection Molding
  • Moisture Content, ISO 15512
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.