MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik VESTAMID® LC-GF30 BK Nylon 12, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 30% Glass Fiber Filled

Material Notes: VESTAMID® LC-GF30 BK is a semi-crystalline, heat- and UV-stabilized compound based on PA 12 from which connectors are preferrably produced by injection molding. The polyamide compound is especially suitable for the automotive and mobility sector. The semi-crystalline molding compound absorbs only small amounts of water. Components made from VESTAMID® LC-GF30 BK therefore have excellent dimensional accuracy with changing ambient humidity and constant general chemical stability. The semi-crystalline polymer is characterized by its outstanding mechanical and thermal load capacity. Molding or process-specific deviations from the recommended processing parameters are possible to a certain extent if the cavity or the process requires it. VESTAMID® LC-GF30 BK is delivered as cylindrical-granules in ready-to-process condition, in moisture-tight packaging.
Dry properties listed below
Industrial Sector: Automotive and Mobility, Industry and Engineering
Processing: Injection molding
Delivery form: Pellets, Granules
Optics: Laser absorbing
Resistance to: Heat (thermal stability), UV / light / weathering
Electrical: Insulating
Conformity: Automotive
Additives: Glass fibers
Applications: Quick-connectors
Special Characteristics: Halogen-free, Semi-crystalline, U.V. stabilized, Medium viscosity
Features: Lightweight, Non-corrosive
Color: Black
Additives: Light stabilizer
Delivery form: Cylindrical pellets
Chemical Resistance: Fuel resistance

Information provided by Evonik.

Vendors:
Available Properties
  • Density, ISO 1183
  • Viscosity Number, ISO 307, 1157, 1628, Corrected
  • Linear Mold Shrinkage, Flow, ISO 294-4, 2577
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 2577
  • Melt Flow, ISO 1133
  • Spiral Flow, Cross Section 6 x 2 mm2
  • Spiral Flow
  • Hardness, Shore D, ISO 7619-1
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527, Nominal
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Tensile Modulus, ISO 527
  • Charpy Impact Unnotched, ISO 179/1eU, Type of failure: C
  • Charpy Impact Unnotched, ISO 179/1eU, Type of failure: C
  • Charpy Impact Unnotched, ISO 179/1eU, Type of failure: C
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Melting Point, ISO 11357-1/-3
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Vicat Softening Point, ISO 306, 50 K/h
  • Vicat Softening Point, ISO 306, 50 K/h
  • Glass Transition Temp, Tg, ISO 11357-1/-2
  • Feed Temperature
  • Nozzle Temperature, Injection Molding
  • Zone 1, Injection Molding
  • Zone 2, Injection Molding
  • Zone 3, Injection Molding
  • Zone 4, Injection Molding
  • Melt Temperature, flow spiral
  • Melt Temperature, Injection Molding
  • Melt Temperature
  • Mold Temperature, flow spiral
  • Mold Temperature, Injection Molding
  • Mold Temperature
  • Injection Velocity, flow front, flow spiral
  • Drying Temperature, Pre-drying
  • Dry Time, Pre-drying
  • Moisture Content, ISO 15512
  • Moisture Content, Processing Humidity
  • Injection Pressure, flow spiral
  • Injection Pressure, flow spiral
  • Hold Pressure, Injection Molding
  • Back Pressure, Injection Molding
  • Screw Speed, Injection Molding
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.