MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Tra-Con Tra-Cast 3145 Thermally Conductive Electrically Insulating Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-CAST 3145 is a medium viscosity thermally conductive epoxy adhesive that is used for staking and setting transistors, diodes, resistors, integrated circuits and other heat-sensitive components in printed circuit electronic applications. This two-part compound develops strong, durable high-impact bonds at room temperature which improve heat transfer while maintaining electrical insulation. TRA-CAST 3145 bonds readily to itself, and to metals, silica, steatite, alumina sapphire and other ceramics, glass, plastics and many other materials, because its coefficient of thermal expansion provides a good match for those materials over a fairly wide temperature range. Fully cured TRA-CAST 3145 provides excellent resistance to salt solutions, mild acids and alkalis, many other chemicals including petroleum solvents, lubricating oils, and alcohol. This adhesive complies with the requirements of NASA Outgassing Specification when tested according to ASTM E-595-90.

Information provided by Tra-Con Inc.

Vendors:
Available Properties
  • Specific Gravity, Mixed
  • Solids Content, Reactive Solids Content
  • Volatile Organic Compounds (VOC) Content
  • Water Absorption, After 24 hours
  • Viscosity, Mixed (rv #6, 10 rpm)
  • Hardness, Shore D
  • Adhesive Bond Strength, Lap shear, alum to alum, 24 hrs @ 25°C
  • Adhesive Bond Strength, Lap shear, alum to alum, 4 hrs @ 25°C + 2 hrs @ 65°C
  • Volume Resistivity
  • Volume Resistivity
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, Ultimate Tg
  • Cure Time, 4 hrs @ 25°C + 2 hrs @ 65°C
  • Cure Time
  • Cure Time
  • Pot Life, 25 grams
  • Pot Life, 100 grams
  • Working Life, 200 grams
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Tra-Con, Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.