MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.
Ensinger TECAPEI® 20% Glass Reinforced, made from Ultem® 2200 PEI
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 20% Glass Fiber

Material Notes: TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in color, and combine exceptional mechanical, thermal, and electrical properties. The addition of glass fiber reinforcement in the 2000 series, coupled with Ensinger's proprietary extrusion techniques, provides the TECAPEI™ with both greater tensile strength and rigidity, while also improving dimensional stability.

  • Excellent mechanical strength (exhibits high tensile strength at room temperature and retains a significant portion of this strength at elevated temperatures. Glass fibers further increase high-temperature strength)
  • Outstanding heat resistance (retains its physical properties at elevated temperatures)
  • Exceptional resistance to environmental forces (Environmental characteristics of TECAPEI™ include it's stress resistance)
  • Inherent flame resistance with low smoke evolution (Tested internally to UL 94 V-0)
  • High mechanical strength
  • High dielectric strength and stability
  • Low dissipation factor over a wide range of frequencies
  • Excellent machinability and finishing characteristics (TECAPEI™ can be easily machined with conventional metalworking tools, painted, hot stamped, printed, or metallized)
  • Resin used in natural grade are FDA, USP Class VI and NSF compliant

TECAPEI™ has many applications in medical, electronic/electrical, microwave, automotive, and aircraft industries.

Information Provided by Ensinger Inc.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570
  • Water Absorption at Saturation, ASTM D570
  • Hardness, Rockwell M, ASTM D785
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Shear Strength, Ultimate
  • Izod Impact, Notched, ASTM D256
  • Volume Resistivity, ASTM D257, 1/16''
  • Dielectric Constant, ASTM D150, 50% RH
  • Dielectric Strength, ASTM D149, In Oil
  • Dissipation Factor, ASTM D150, 50% RH
  • CTE, linear, Parallel to Flow, ASTM D696
  • Thermal Conductivity, ASTM D2214
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, 1/4''
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, 1/4''
  • Flammability, UL94
  • USP Class VI
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

USP Class VI adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.