MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Raschig Group 5553 DAP
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled; Filled/Reinforced Thermoset

Material Notes: Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensional stability even under severe environmental condition. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS)

Processing: Compression and transfer molding

Applications: Connectors, Bobbins, Potentiometers, switches

Information provided by the Raschig Group

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Apparent Bulk Density, ISO 60
  • Water Absorption, ISO 62
  • Linear Mold Shrinkage, ISO 2577, Injection
  • Linear Mold Shrinkage, ISO 2577
  • Tensile Strength, Yield, ISO 527, Compression
  • Tensile Strength, Yield, ISO 527, Injection
  • Modulus of Elasticity, ISO 527, Compression
  • Modulus of Elasticity, ISO 527, Injection
  • Flexural Strength, ISO 178, Compression
  • Flexural Strength, ISO 178, Injection
  • Flexural Modulus, ISO 178, Compression
  • Flexural Modulus, ISO 178, Injection
  • Compressive Strength, ISO 604
  • Charpy Impact Unnotched, ISO 179/ 1eU, Compression
  • Charpy Impact Unnotched, ISO 179/ 1eU, Injection
  • Charpy Impact, Notched, ISO 179/ 1eA, Compression
  • Charpy Impact, Notched, ISO 179/ 1eA, Injection
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, IEC 60112
  • CTE, linear, ISO 11359-2
  • Thermal Conductivity, ASTM E1461
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-A, Compression
  • Deflection Temperature at 8.0 MPa, ISO 75-C
  • Flammability, UL94
  • Shrinkage, ISO 2577, Post shrinkage
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.