MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Lanxess LEWATIT® K 2629 Polymer-based Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® K 2629 is a strongly acidic, macroporous, polymer-based resin in spherical bead form, with sulfonic acid groups. It is ideal suited as a heterogeneous catalyst for organic reactions and for the processing of aqueous and organic liquids. A large pore structure, high degree of crosslinking and good mechanical stability enable this catalyst to be used in polar and non-polar media. It is very compact and thus of exceptional mechanical stability. Therefore, it is especially suitable for use in the following applications:
  • Production of the gasoline additives MTBE, ETBE and TAME
  • Phenol alkylations and transalkylations, hydration of olefins, esterification, etherification, condensation and alkylation of larger polar and non-polar molecules
  • Cation removal, base adsorption from aqueous and organic liquids.

Information provided by Lanxess.

Vendors:
Available Properties
  • Bulk Density
  • Density
  • Bead Size, >90%
  • Storage Temperature
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lanxess, Spinoff of Bayer

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.