MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
DuPont™ Kapton® 50FPC Polyimide Film, 13 Micron Thickness
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: Film thickness 13 micron (0.5 mil)

All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).

General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dianhydride with an aromatic diamine. It has excellent chemical resistance; there are no known organic solvents for the film. It does not melt. It can be used at both high and low temperature extremes. Kapton® polyimide films can be used in a variety of electrical and electronic uses: wire and cable tapes, formed coil insulation, substrates for printed circuit boards, motor slot liners, magnet wire insulation, transformer and capacitor insulation, magnetic and pressure-sensitive tapes, and tubing.

Data provided by DuPont High Performance Films.

Vendors:
Available Properties
  • Density
  • Water Absorption, 24 hr/23°C. ASTM D570
  • Thickness
  • Film Elongation at Break, MD, ASTM D882, Orientation not specified
  • Poissons Ratio, Value for Kapton® HN
  • Secant Modulus, ASTM D882
  • Coefficient of Friction, Dynamic, Value for Kapton® HN. Film to film. ASTM D1894-90
  • Coefficient of Friction, Static, Kapton® HN. Film to film. ASTM D1894-90
  • Film Tensile Strength at Break, MD, ASTM D882, Orientation not specified
  • Electrical Resistivity, Kapton® HN in damp heat; IPC-TM-650; Method 2.5.17
  • Electrical Resistivity, per ASTM D257-91 for Kapton® HN
  • Dielectric Constant, ASTM D150, Use evaporated metal electrodes, two terminal system of measurement at standard conditions.
  • Dielectric Strength, ASTM D149-81, Flat sheets in air; 1/4 in diameter brass electrodes with 0.8 mm edge radius; 60 cps AC at 600V/s
  • Dissipation Factor
  • CTE, linear, Value for Kapton® HN
  • CTE, linear, Value for Kapton® HN
  • CTE, linear, Value for Kapton® HN
  • Specific Heat Capacity, Value for Kapton® HN
  • Thermal Conductivity, Value for Kapton® HN
  • Maximum Service Temperature, Air, Kapton® can function after brief exposure to 400°C (750°F). Various grades are UL rated for continuous service at 220-240°C (430-460°F).
  • Minimum Service Temperature, Air, Maintains properties and flexibility
  • Glass Transition Temp, Tg, Value for Kapton® HN
  • Flammability, UL94
  • Refractive Index, ASTM D542-90, Value for Kapton® HN.  Na D line
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.