MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Akro-Plastic Akromid® C3 GF 25 1 FR black (7246) Nylon 66/6, 25% Glass Fiber, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: Flame Retardant Compound. V0, good GWFI, easy flow, good strain at break. PA 6.6 + PA 6 GF 25 FR (40).

Information provided by Akro-Plastic GmbH

Vendors:
Available Properties
  • Density, ISO 1183
  • Filler Content, ISO 1172
  • Linear Mold Shrinkage, Flow, ISO 294-4
  • Linear Mold Shrinkage, Transverse, ISO 294-4
  • Tensile Strength at Break, ISO 527-2, 5 mm/min. Conditioned
  • Tensile Strength at Break, ISO 527-2, 5 mm/min. Dry as Molded
  • Elongation at Break, ISO 527-2, 5 mm/min. Dry as Molded
  • Elongation at Break, ISO 527-2, 5 mm/min. Conditioned
  • Tensile Modulus, ISO 527-2, 1 mm/min. Conditioned
  • Tensile Modulus, ISO 527-2, 1 mm/min. Dry as Molded.
  • Flexural Strength, ISO 178, Conditioned. 2 mm/min
  • Flexural Strength, ISO 178, Dry as Molded. 2 mm/min
  • Flexural Modulus, ISO 178, 2 mm/min. Conditioned
  • Flexural Modulus, ISO 178, 2 mm/min. Dry as Molded
  • Charpy Impact Unnotched, ISO 179-1/1eA, Dry as Molded
  • Charpy Impact Unnotched, ISO 179-1/1eA, Conditioned
  • Charpy Impact, Notched, ISO 179-1/1eA, Dry as Molded
  • Charpy Impact, Notched, ISO 179-1/1eA, Conditioned
  • Dielectric Strength, IEC 60243, Conditioned
  • Dielectric Strength, IEC 60243, Dry as Molded
  • Comparative Tracking Index, IEC 60112, Dry as Molded. Test solution A.
  • Hot Wire Ignition, HWI, UL 746A, Conditioned
  • Hot Wire Ignition, HWI, UL 746A, Conditioned
  • Hot Wire Ignition, HWI, UL 746A, Conditioned
  • Hot Wire Ignition, HWI, UL 746A, Conditioned
  • Hot Wire Ignition, HWI, UL 746A, Dry as Molded
  • Hot Wire Ignition, HWI, UL 746A, Dry as Molded
  • Hot Wire Ignition, HWI, UL 746A, Dry as Molded
  • Hot Wire Ignition, HWI, UL 746A, Dry as Molded
  • High Amp Arc Ignition, HAI, UL 746A, Conditioned
  • High Amp Arc Ignition, HAI, UL 746A, Conditioned
  • High Amp Arc Ignition, HAI, UL 746A, Conditioned
  • High Amp Arc Ignition, HAI, UL 746A, Conditioned
  • High Amp Arc Ignition, HAI, UL 746A, Dry as Molded
  • High Amp Arc Ignition, HAI, UL 746A, Dry as Molded
  • High Amp Arc Ignition, HAI, UL 746A, Dry as Molded
  • High Amp Arc Ignition, HAI, UL 746A, Dry as Molded
  • Melting Point, DIN EN 11357-1, Dry as Molded. DES, 10°C/min
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75, Dry as Molded
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75, Dry as Molded
  • UL RTI, Electrical, UL 746 B, Conditioned
  • UL RTI, Electrical, UL 746 B, Conditioned
  • UL RTI, Electrical, UL 746 B, Conditioned
  • UL RTI, Electrical, UL 746 B, Conditioned
  • UL RTI, Electrical, UL 746 B, Dry as Molded
  • UL RTI, Electrical, UL 746 B, Dry as Molded
  • UL RTI, Electrical, UL 746 B, Dry as Molded
  • UL RTI, Electrical, UL 746 B, Dry as Molded
  • UL RTI, Mechanical with Impact, UL 746 B, Conditioned
  • UL RTI, Mechanical with Impact, UL 746 B, Conditioned
  • UL RTI, Mechanical with Impact, UL 746 B, Conditioned
  • UL RTI, Mechanical with Impact, UL 746 B, Conditioned
  • UL RTI, Mechanical with Impact, UL 746 B, Dry as Molded
  • UL RTI, Mechanical with Impact, UL 746 B, Dry as Molded
  • UL RTI, Mechanical with Impact, UL 746 B, Dry as Molded
  • UL RTI, Mechanical with Impact, UL 746 B, Dry as Molded
  • UL RTI, Mechanical without Impact, UL 746 B, Conditioned
  • UL RTI, Mechanical without Impact, UL 746 B, Conditioned
  • UL RTI, Mechanical without Impact, UL 746 B, Conditioned
  • UL RTI, Mechanical without Impact, UL 746 B, Conditioned
  • UL RTI, Mechanical without Impact, UL 746 B, Dry as Molded
  • UL RTI, Mechanical without Impact, UL 746 B, Dry as Molded
  • UL RTI, Mechanical without Impact, UL 746 B, Dry as Molded
  • UL RTI, Mechanical without Impact, UL 746 B, Dry as Molded
  • Flammability, UL94, Conditioned
  • Flammability, UL94, Conditioned
  • Flammability, UL94, Conditioned
  • Flammability, UL94, Conditioned
  • Flammability, UL94, Dry as Molded
  • Flammability, UL94, Dry as Molded
  • Flammability, UL94, Dry as Molded
  • Flammability, UL94, Dry as Molded
  • Glow Wire Ignition Temperature, IEC 60695-2-13, Conditioned
  • Glow Wire Ignition Temperature, IEC 60695-2-13, Conditioned
  • Glow Wire Ignition Temperature, IEC 60695-2-13, Conditioned
  • Glow Wire Ignition Temperature, IEC 60695-2-13, Conditioned
  • Glow Wire Ignition Temperature, IEC 60695-2-13, Dry as Molded
  • Glow Wire Ignition Temperature, IEC 60695-2-13, Dry as Molded
  • Glow Wire Ignition Temperature, IEC 60695-2-13, Dry as Molded
  • Glow Wire Ignition Temperature, IEC 60695-2-13, Dry as Molded
  • Glow Wire Flammability Index, IEC 60695-2-12, Conditioned
  • Glow Wire Flammability Index, IEC 60695-2-12, Conditioned
  • Glow Wire Flammability Index, IEC 60695-2-12, Conditioned
  • Glow Wire Flammability Index, IEC 60695-2-12, Conditioned
  • Glow Wire Flammability Index, IEC 60695-2-12, Dry as Molded
  • Glow Wire Flammability Index, IEC 60695-2-12, Dry as Molded
  • Glow Wire Flammability Index, IEC 60695-2-12, Dry as Molded
  • Glow Wire Flammability Index, IEC 60695-2-12, Dry as Molded
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.