MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SSAB Toolox® 44 Steel
Categories: Metal; Ferrous Metal; Carbon Steel

Material Notes: Toolox 44 is a steel already heat treated to the final properties. Thus saving time, costs and risks associated with heat treatment. The very high strength is combined with a high and guaranteed toughness as well as an excellent fatigue resistance. Making Toolox 44 the ideal choice for the most demanding engineering and mold and die applications. Toolox 44 can be surface hardened with methods like nitriding, laser and induction. Giving the possibilities to even further improve the performance.

Dimension Range: Toolox 44 is available as plates in thicknesses between 6.0 - 130.0 mm, and as forged block in thickness up to 320 mm.

Data provided by SSAB.

Vendors:
Available Properties
  • Hardness, Brinell
  • Hardness, Brinell
  • Tensile Strength, Rm
  • Tensile Strength, Yield, Rp0.2
  • Elongation at Break, A5
  • Charpy Impact, 10x10 mm test specimen, longitudinal
  • Charpy Impact, 10x10 mm test specimen, longitudinal
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
SSAB Tunnplat AB

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.