MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Dow Dow™ DGDA-2485 NT HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Industrial Standard Compliance: ASTM D 3350: cell classification PE445520A (See NOTES 1); American Association of State Highway and Transportation Officials (AASHTO) M294/MP7 (See NOTES 2) DOW DGDA-2485 NT High Density Polyethylene resin is produced using UNIPOL™ II process technology and meets the needs of a wide variety of end uses including profile extrusion applications such as corrugated pipe. It combines excellent ESCR/NCLS with superior toughness and processability.
NOTES: (1) The first five numbers of the cell classification are based on natural resin. The last number and letter are based on black resin (natural resin plus 6.5% DFNF-0092). (2)Natural resin extruded under proper conditions with carbon black masterbtach DFNF-0092 (6.5%)

Availability: Asia Pacific; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: AASHTO M294/MP7; ASTM D3350 PE346460A

Form: Pellets

Processing Method: Profile Extrusion

Information provided by The Dow Chemical Company

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Melt Flow, ASTM D1238
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break
  • Flexural Modulus, ASTM D790B, 2% Secant, Method I (3 point load)
  • Tensile Impact Strength, ASTM D1822, Type S
  • Melting Point
  • Brittleness Temperature, ASTM D746
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.