MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Go Yen Chemical Electric Welding Rod TiO2 Titanium Dioxide
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Advantages:
  • isolating air
  • protecting melted metal
  • preventing air entrance
  • Deoxidizing
  • denitrifying
  • reforming mechanical property
  • Adding alloy element
  • Stabilized
  • Propitious to vertical-position welding
  • Arcing fast
  • Little Impurity contentontent
  • produce cold seam
  • Granule is small and average, sieved remaining of 45µm sieve pore should be less 0.5%
Applications:
  • welding rod
  • Slag-making agent, with excellent deoxidization effect
  • well welding thinner, adhesive, arc stabilizer
  • applied on alternating current
  • direct current welding rods
  • reduce SO2 consumption during produced process, making surface smooth, make arc easily
  • Other application of specific industry products.

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Density
  • Oil Absorption
  • Particle Size, 0.1% Residue
  • pH, Water Suspension
  • Moisture Content
  • TiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.